💰 INSCRIVEZ-VOUS ET PROFITEZ DE €8 DE RÉDUCTION SUR VOTRE PREMIÈRE COMMANDE

📦 POUR UNE DURÉE LIMITÉE LIVRAISON GRATUITE SUR TOUTES LES COMMANDES

Achetez plus, économisez plus !

Économisez jusqu’à 50% + un cadeau surprise gratuit pour les commandes éligibles.

Acheter maintenant

Collection Nylon


  • Fiberon™ PA12-CF10

  • Fiberon™ PA6-CF20

  • Fiberon™ PA6-GF25

  • Fiberon™ PA612-CF15

  • Fiberon™ PA612-ESD

  • Fiberon™ PPS-GF20

  • Épuisé

    PolyMide™ CoPA

haute Résistance aux chocs + Haute résistance à la chaleur

Matériau d'ingénierie Pour 3D imprimé

Le PA - qui signifie nylon polyamide - est une option de matériau d’impression 3D très résistante.

Résistance aux chocs élevéeHaute résistance à la chaleurEngineering

FAQ sur Nylon

Qu’est-ce que le filament de nylon ?

Nylon filament is a family of polyamide engineering thermoplastics used for FDM/FFF 3D printing. A nylon 3D printer filament is typically chosen for tough, wear-resistant functional parts such as gears, bushings, brackets, jigs, and fixtures. Unlike many general-purpose 3D printing filaments, PA filament absorbs moisture readily and must be stored and printed under dry conditions.

Quel type de filament de nylon convient le mieux à mon projet ?

The best nylon printer filament depends on the required strength, stiffness, humidity resistance, and electrical properties:

  • PolyMide CoPA is a Nylon 6/6,6 copolymer for tough, heat-resistant engineering parts.
  • Fiberon PA6-CF20 provides high strength, stiffness, and heat resistance but is more sensitive to moisture than PA12 or PA612.
  • Fiberon PA6-GF25 is suitable when high layer adhesion, stiffness, and impact resistance are priorities.
  • Fiberon PA12-CF10 has the lowest moisture absorption in the range and provides good dimensional stability in humid conditions.
  • Fiberon PA612-CF15 balances high mechanical performance with lower moisture absorption than PA6.
  • Fiberon PA612-ESD is designed for static-dissipative parts used around sensitive electronics.

Choose the nylon 3D filament whose technical data matches the part’s load, operating temperature, humidity, and electrical requirements.

Quelle est la différence entre les filaments de nylon PA6, PA12 et PA612 ?

The main differences are moisture absorption, dimensional stability, and mechanical performance:

  • PA6: Provides strong mechanical and thermal performance but absorbs more moisture, which can cause greater changes in dimensions and material properties.
  • PA12: Absorbs less moisture than PA6 and maintains more consistent dimensions and mechanical properties in humid environments.
  • PA612: Falls between PA6 and PA12 in moisture resistance, mechanical properties, and price.

The reinforcement type and fiber percentage can affect performance as much as the base PA filament, so compare the complete product TDS rather than selecting by the PA number alone.

Quelle est la différence entre le nylon renforcé de fibres de carbone et le nylon chargé de verre ?

Both carbon fiber nylon filament and glass filled nylon contain short reinforcing fibers that improve stiffness, heat resistance, and dimensional stability. Carbon-fiber grades are generally lighter and provide high specific stiffness with a black, matte surface, while glass-fiber grades are denser and may provide different impact and layer-adhesion characteristics.Neither reinforcement is automatically stronger in every direction. Compare the XY and Z-axis properties in the product TDS when choosing a fiber-reinforced filament for a load-bearing part.

Le filament de nylon nécessite-t-il une Imprimante 3D fermée ?

An actively heated enclosure is not required for these Polymaker nylon materials. Fiberon nylon grades specify a room-temperature chamber, while the current PolyMide CoPA TDS specifies a closed chamber at ambient temperature; a passive, unheated enclosure is therefore appropriate for CoPA.For a reliable nylon filament 3D print, keeping the material dry and using a hotend that reaches the specified temperature are more important than heating the chamber. Polymaker’s Warp-Free™ process also requires the build environment to remain below 50°C.

Quels Paramètres d'impression dois-je utiliser pour le filament de nylon Polymaker ?

Polymaker nylon 3D printer filament should be printed dry with the cooling fan turned off and an all-metal hotend rated for the required temperature. Most Fiberon nylon grades use a 280–300°C nozzle and a 40–50°C build plate; Fiberon PA612-CF15 uses 250–300°C, while PolyMide CoPA uses a 250–270°C nozzle and a 25–50°C build plate. Because nozzle requirements and suitable printing speeds vary by product and printer, follow the profile provided for the selected filament.

Le filament de nylon doit-il être séché avant l’impression ?

Yes. Nylon filament is highly hygroscopic, and absorbed moisture can cause popping, excessive stringing, rough surfaces, inconsistent extrusion, and weak layers. Polymaker specifies the following drying conditions:

  • Fiberon PA6, PA12, and PA612 grades: 100°C for 10 hours.
  • PolyMide CoPA: 100°C for 8 hours according to the current TDS.

Store and print these materials below 20% relative humidity whenever possible, preferably feeding the filament directly from a dry box or heated filament dryer. PA12 absorbs less moisture than PA6, but it should still be kept dry.

Le nylon renforcé de fibres de carbone et le nylon chargé de verre nécessitent-ils une Buse durcie ?

Yes. A nylon carbon fiber filament or glass-fiber-reinforced nylon can wear a standard brass nozzle rapidly. Polymaker specifies a wear-resistant nozzle—such as hardened steel or ruby—with a diameter of at least 0.4 mm for its Fiberon CF and GF nylon products.Fiberon PA612-ESD also requires a hardened nozzle because it contains carbon reinforcement. Although PolyMide CoPA is not labeled as a CF or GF grade, its current TDS also highly recommends a wear-resistant nozzle because brass-nozzle abrasion can occur.

Comment éviter le gauchissement ou une perte d’Adhérence entre les couches lors de l’impression de filament de nylon ?

For a successful nylon filament 3D print:

  • Dry the filament and continue feeding it from a dry environment during printing.
  • Use the specified nozzle-temperature range and keep the cooling fan off.
  • Set the bed to 40–50°C for Fiberon nylon or 25–50°C for PolyMide CoPA.
  • Apply a glue stick or a nylon-specific adhesive such as Magigoo PA if bed adhesion is weak.
  • Keep the build area free from drafts without using a chamber temperature above 50°C.

If layers separate, confirm that the filament is dry before increasing the nozzle temperature within the approved range or reducing print speed.

Les pièces imprimées avec du filament en nylon doivent-elles subir un recuit après l’impression ?

Annealing is recommended when the finished part must achieve the thermal and mechanical performance stated for the annealed material. It may be unnecessary for a visual prototype, but it is important for demanding functional parts.

  • Fiberon PA6, PA12, and PA612 grades: Anneal at 100°C for 16 hours.
  • PolyMide CoPA: Anneal at 80°C for 6 hours.

Annealing a nylon printer filament part can cause dimensional changes, so test the process before treating a precision component. Because annealing dries the part, moisture conditioning should be performed afterward when the application or validation procedure requires a moisture-conditioned state.